Ingredients: The mixture consists of a combination of gypsum and calcium carbonate, as well as cellulose additives, which regulate the bonding process during the work.
Surface preparation and use: Carry out the work at an air temperature of not less than +10˚C and a relative humidity of not more than 75%. Gradually add dry mortar to room temperature water, mix with a mixer until a homogeneous mass is obtained. Leave the mortar to mature for 5-7 minutes, mix again before use. Perform the work with a stainless spatula (spatula). First clean the surface from dust, dirt, other unstable formations (e.g. remnants of old wallpaper, oil paint, etc.), eliminate weak areas of the base, making the surface as load-bearing as possible. Expand small cracks by filling them in advance before the general layer. If necessary, it is recommended to use a liquid primer. After complete drying, to obtain a smoother surface, it is necessary to sand the surface. After completing the work, wash the tools with water. Dispose of used bags and mortar residues in accordance with the established procedure.
Optimal layer thickness: from 0.8 mm to 3 mm.
Mixture viability: 60-70 minutes.
Consumption: 10kg-11kg /10m² (at a layer thickness of 1mm).
Water consumption: 15-17l. for 30kg (about 520ml for 1kg of dry mortar).